Nitronic
Aluia maualuga le vevela
◆Nitronic50 (S20910 / XM-19) o se uʻamea austenitic faʻaleleia nitrogen, lea e masani ona faʻaaogaina i le petrochemical, textile, gaosiga o meaʻai ma alamanuia o le gataifale.
◆Nitronic60 (S21800 / Alloy218) e sili ona lelei le maualuga o le vevela o le faʻamaʻiina o le faʻamaʻiina o le faʻamaʻiina ma le maualalo o le vevela o aʻafiaga, ma e masani ona faʻaaogaina i pine alalaupapa alalaupapa faʻamaʻi ma isi galuega autu.
Su'ega vaila'au
Vasega | C | Si | Mn | S | P | Cr | Ni | Fe | Mo | Ti | Cu | Nb | N | isi |
e le sili atu | ||||||||||||||
Nitronic50 | 0.06 | 1 | 4~6 | 0.03 | 0.04 | 20.5~23.5 | 11.5~13.5 | faavae | 1.5~3 | - | - | 0.1~0.3 | 0.2~0.4 | - |
Nitronic60 | 0.1 | 3.5~4.5 | 7~9 | 0.03 | 0.04 | 16–18 | 8~9 | faavae | — | — | — | — | 0.08~0.18 | - |
Alloy mea totino aupito maualalo
Vasega | setete | malosi mālosi RmN/m㎡ | Malosi fua Rp0.2N/m㎡ | Elongation As% | Brinell malo HB |
Nitronic50 | Fofo togafitiga | 690 | 380 | 35 | - |
Nitronic60 | Fofo togafitiga | 600 | 320 | 35 | - |