Alu Sa'o Maualuga
Aluia maualuga le vevela
◆1J50 o loʻo i ai se matasele hysteresis rectangular ma maualuga saturation maneta induction.E masani ona fa'aaogaina i mea fa'amalo fa'amaneta, coils choke, coils fa'asa'o, ma vaega masini komepiuta o lo'o galue i totonu ole fanua maneta.
◆1J79 o loʻo i ai le maualuga muamua o le maneta, ma e talafeagai mo transformers eseese, transformers, amplifiers mageta, cores maneta ma talipupuni faʻamaneta o loʻo galue i fanua maneta vaivai.
◆3J53 o loʻo i ai le maualuga o le vevela o le vevela i le va o le -40-80 ° C, ma faʻaaogaina mo le vibrator i le masini masini, le ofe o le vibration relay ma isi vaega.
◆4J29(F15) o loʻo i ai le faʻalauteleina o le faʻalauteleina o le vevela laina tutusa ma le tioata malo i totonu o se vaega o le vevela, ma e faʻaaogaina mo le fetaui ma tioata malo i totonu o le alamanuia gaogao.
◆4J36 o se faʻapitoa faʻapitoa faʻalauteleina uʻamea-nickel faʻatasi ma le ultra-low le faʻalauteleina o le faʻalauteleina, lea e faʻaaogaina i le siosiomaga e manaʻomia ai le faʻalauteleina o le faʻalauteleina.
◆4J42 e masani ona faʻaaogaina i le gaosiga o masini eletise eletise, mea faʻapitoa, mea faʻaoga faʻasolosolo faʻasolosolo ma manaʻoga mautu maualuga, ma isi.
Su'ega vaila'au
Vasega | C | Si | Mn | S | P | Cr | Ni | Mo | Cu | Fe | Al | Co | Ti |
e le sili atu | |||||||||||||
1J50 | 0.03 | 0.15~0.3 | 0.3~0.6 | 0.02 | 0.02 | - | 49.5~50.5 | - | ≤0.2 | faavae | — | — | — |
1J79 | 0.03 | 0.3~0.5 | 0.6~1.1 | 0.02 | 0.02 | - | 78.5~80.5 | 3.8~4.1 | ≤0.2 | faavae | — | — | — |
3J53 | 0.05 | 0.8 | 0.8 | 0.02 | 0.02 | 5.2~5.8 | 41.5~43 | 0.7~0.9 | — | faavae | 0.5~0.8 | — | 2.3~2.7 |
4J29 | 0.03 | 0.3 | 0.5 | 0.02 | 0.02 | <0.2 | 28.5~29.5 | <0.2 | ≤0.2 | faavae | — | 16.8~17.8 | — |
4J36 | 0.05 | 0.3 | 0.2~0.6 | 0.02 | 0.02 | - | 35–37 | - | — | faavae | — | — | — |
4J42 | 0.05 | 0.3 | 0.8 | 0.02 | 0.02 | - | 41.5~42.5 | — | — | faavae | ≤0.1 | ≤1.0 | - |
Alloy mea totino aupito maualalo
Vasega | Eseesega | Mea fa'amaneta | ||
Ulua'i fe'avea'i uo(MH/m) | Maualuluga Maumea(Uh/m) | Fa'amalosi Hc(A/m) | ||
1J79 | Ta'ai malulu | ≥31 | ≥250 | ≤1.2 |
laupapa uaea laau | ≥25 | ≥125 | ≤2.4 | |
1J50 | Ta'ai malulu | ≥3.8 | ≥62.5 | ≤9.6 |
Fa'amau (taai) fa'amau | ≥3.1 | ≥31.3 | ≤14.4 |
Vasega | setete | Elastic Modulus E(Mpa) | malosi mālosi b(N/m㎡) | Malosi Hv |
3J53 | galue malulu + matua | 190000~215600 | 1170~1760 | 400~480 |
Vasega | Fuafuaga Fa'atele Fa'atele (10-6℃) | ||||||
20~100℃ | 20~300℃ | 20~400℃ | 20~450℃ | 20~500℃ | 20~530℃ | 20~600℃ | |
4J29 | — | — | 4.6~5.2 | 5.1~5.5 | — | — | — |
4J50 | — | 9.2~10 | 9.2~9.9 | — | — | — | — |
4J36 | — | ≤1.5 | — | — | — | — | — |
4J42 | 5.5 | 4.6 | 5.8 | 6.7 | 7.6 | — | 9.1 |