◆GH2132 (incoloyA-286/S66286) o loʻo i ai le lelei o le faʻatinoga atoa ma le maualuga o le fua. E fa'aaogaina mo tisiki turbine, tino mama, fa'amau fa'amau ma mea tau vaega i lalo ole 700 °C.
◆GH3030 alloy o loʻo i ai se fausaga mautu, faʻaitiitia le matua, ma le lelei o le faʻamaʻiina. E talafeagai mo potu mu ma afterburers i lalo ole 800 °C.
◆GH3128 o loʻo i ai le lelei atoatoa o faʻatinoga, maualuga le tumau, faʻamaʻiina lelei o le faʻamaʻiina, lelei le faʻatulagaina ma le lelei o le faʻaogaina o galuega, ma e masani ona faʻaaogaina mo le potu faʻafefe ma vaega afterburner o le afi turbine ma le vevela galue o le 950 ° C
◆GH4145 (inconelx-750 / N07750) e lava le malosi, faʻamaʻi faʻamaʻi ma faʻamaʻiina i lalo ole 980 ° C. O le mea e sili ona fiafia i ai mo puna maualuga-malosi ma e talafeagai mo le faia o diaphragms elastic ma faʻamau faʻamaufaʻailoga.
◆GH4169 (N07718/inconel718) o loʻo i ai se fausaga austenite, ma o le vaega "Y" na fausia ina ua maeʻa le faʻamaʻaina o timuga e maua ai le lelei o mea faʻainisinia. E masani ona faʻaaogaina i nofoaga eseese e manaʻomia le maualuga o le vevela.
◆GH4080A (N07080 / Nimonic80A) Z ua lava le vevela maualuga i le 700-750 ° C ma le lelei o le okesene tetee i lalo ole 900 ° C. O lenei uʻamea faʻapitoa e fetaui lelei mo fanua e manaʻomia ai le malosi maualuga ma le faʻafefe.
◆GH3044 O le potu faʻafefeteina autu ma vaega afterburner, talipupuni vevela, taʻiala taʻiala, ma isi.
◆GH4080A o loʻo i ai le malosi o le fetolofi ma le faʻamaʻiina o le faʻamaʻiina i le va o le 650-850 ° C.
◆GH2136 o loʻo i ai le lelei atoa o le faʻatinoga, faʻamautu fausaga pe a uma le faʻaaogaina umi, faʻamaʻi faʻamaʻi lelei, faʻasolosolo faʻalauteleina laina, ma faigofie le faʻapipiʻiina ma le fausiaina.
◆GH2036 Tiki Turbine, talipupuni vevela, mama faʻamau, mama faʻamau, faʻamau, ma isi mea e galue i lalo ole 650 °C.
◆GH4738 e talafeagai mo le faia o tisiki turbine, lau galuega, faʻamau maualuga-vevela, paipa afi, uʻamea ma turbines, ma isi.
Fa'ameamea
Vasega | C | Si | Mn | S | P | Cr | Co | W | Mo | Ti | Al | Fe | Ni | isi |
e le sili atu | ||||||||||||||
GH2132 | 0.08 | 1 | 2 | 0.02 | 0.03 | 13.5~16 | - | - | 1~1.5 | 1.75~2.35 | ≤0.4 | faavae | 24–27 | B:0.001~0.01 V:0.1~0.5 |
GH3030 | 0.12 | 0.8 | 0.7 | 0.02 | 0.03 | 19–22 | - | - | - | 0.15~0.35 | ≤0.15 | ≤1.5 | faavae | - |
GH3128 | 0.05 | 0.8 | 0.5 | 0.013 | 0.013 | 19–22 | - | 7.5~9 | 7.5~9 | 0.4~0.8 | 0.4~0.8 | ≤2.0 | faavae | B≤0.005 Ce≤0.05 Zr≤0.06 |
GH4145 | 0.08 | 0.5 | 1 | 0.01 | 0.015 | 14~17 | ≤1 | - | - | 2.25~2.75 | 0.4~1 | 5~9 | ≥70 | Nb:0.7~1.2 |
GH4169 | 0.08 | 0.35 | 0.35 | 0.015 | 0.015 | 17–21 | ≤1 | - | 2.8~3.3 | 0.65~1.15 | 0.2~0.8 | Tumau | 50–55 | Cu≤0.3 Nb4.75~5.5 Mg≤0.1 B≤0.006 |
GH4080A | 0.04~0.1 | 1 | 1 | 0.015 | 0.02 | 18–21 | ≤2 | - | - | 1.8~2.7 | 1~1.8 | - | ≥65 | Cu≤2 B≤0.006 |
GH3044 | 0.1 | 0.8 | 0.5 | 0.013 | 0.013 | 23.5~26.5 | — | 13–16 | ≤1.5 | 0.3~0.7 | ≤0.5 | ≤4.0 | faavae | Cu≤0.07 |
GH2136 | 0.06 | 0.75 | 0.35 | 0.025 | 0.025 | 13–16 | — | — | 1~1.75 | 2.4~3.2 | ≤0.35 | faavae | 24.5~28.5 | B:0.005~0.025 V:0.01~0.1 |
GH2036 | 0.34~0.4 | 0.3~0.8 | 7.5~9.5 | 0.03 | 0.035 | 11.5~13.5 | — | — | 1.1~1.4 | ≤0.12 | — | faavae | 7~9 | V:1.25~1.55 Nb:0.25~0.5 |
GH4738 | 0.03~0.1 | 0.15 | 0.1 | 0.015 | 0.015 | 18–21 | 12~15 | — | 3.5~5 | 2.75~3.25 | 1.2~1.6 | ≤2.0 | faavae | B:0.003~0.01 Zr:0.02~0.08 |
Alloy mea totino aupito maualalo
setete | Malosi fa'amalosi RmN/m㎡ | Malosi fua Rp0.2N/m㎡ | Elongation As% | Brinell malo HB |
Fofo togafitiga | 610 | 270 | 30 | ≤321 |
Fofo togafitiga | 650 | 320 | 30 | — |
Fofo togafitiga | 735 | 340 | 40 | — |
Fofo togafitiga | 910 | 550 | 25 | ≤350 |
Fofo togafitiga | 965 | 550 | 30 | ≤363 |
Fofo togafitiga | 845 | 340 | 48.5 | - |
Fofo togafitiga | 920 | 550 | 25 | - |
Fofo togafitiga | 950 | 700 | 20 | - |
Fofo togafitiga | 850 | 600 | 15 | - |
Fofo togafitiga | 1111 | 741 | 21.5 | 24.5 |