Hastelloy C-276 FA'AMATALAGA FAAMATALAGA
Fa'amatalaga o oloa
HT PIPE e maua ai Hastelloy C276 Nickel alloy round bar, Alloy C276 Bar supplier i Saina. 2.4819 pa lapotopoto, Alloy C276 rod, UNS N10276 rod, Alloy C276 flat Bar, Hastelloy C276 pa omo, Hastelloy C276 Nickel alloy round bar supplier, exporter.
O a uiga o Hastelloy C276?
● sili atu le corrosion tetee i le faaitiitia o siosiomaga
● E matuā tetee atu i vaifofo malolosi o masima oxidizing, e pei o ferric ma cupric chlorides
● maualuga nickel ma molybdenum i totonu e maua ai le faʻafefeteina lelei i le faʻaitiitia o siosiomaga
● E maualalo le kaponi i totonu e faʻaitiitia ai le faʻafefe o le carbide o le saito i le taimi o le ueloina e faʻamautu ai le tetee atu i le pala i sone e afaina ai le vevela o sooga uelo.
● Tete'e i a'a fa'apitonu'u e pei ole pitting ma fa'amamafa-corrosion ta'e
● O se tasi o nai mea e mafai ona tetee atu i aafiaga leaga o le kasa chlorine susu, hypochlorite ma chlorine dioxide
Hastelloy C276 u'a nikeli lapotopoto pa u'amea Fa'asu'ega vaila'au,%
Ni | Mo | Cr | Fe | W | Co | Mn | C | V | P | S | Si |
Toega | 15.0-17.0 | 14.5-16.5 | 4.0-7.0 | 3.0-4.5 | 2.5 maualuga | 1.0 maualuga | .01 maualuga | .35 maualuga | .04 maualuga | .03 maualuga | .08 maualuga |
Fa'amatalaga
ASTM faʻamatalaga
Pipa Smls | Uila paipa | Tube Smls | Fa'apa Uila | Pepa/Ipu | Pa | Fa'ailogaina | Fa'atatau | Uaea |
B622 | B619 | B622 | B626 | B575 | B574 | B564 | B366 |
Hastelloy C276 Meatotino faaletino
Liu liusuavai: 1325-1370 ℃
Malosi: 8.90 g/cm3
Alloy C276 Bar Meatotino Fa'ainisinia
Mea tau masini | Tensile, min, ksi[MPa] | Fua, min, ksi[MPa] | Fa'atele, %(min) |
Hastelloy C276 | 100[690] | 41[283] | 40 |
Fa'ata'ita'iga Va'ava'a Va'ava'a Potu o Mea Fa'ama'i
Fomu o oloa | Ta'alo (ksi) | .2% Fua (ksi) | Fa'aumi % |
Pa | 110.0 | 52.6 | 62 |
Papatusi | 107.4 | 50.3 | 67 |
Pepa | 115.5 | 54.6 | 60 |
Paipa & Paipa | 105.4 | 45.4 | 70 |