Hastelloy

  • Hastelloy B

    Hastelloy B o se vaifofo malosi faʻamalosia, nickel-molybdenum alloy, faʻatasi ai ma le tetee tele i le faʻaitiitia o siosiomaga e pei o le hydrogen chloride gas, ma sulfuric, acetic ma phosphoric acids. O le Molybdenum o le elemene faʻafefiloi muamua lea e maua ai le malosi o le pala i le faʻaitiitia o siosiomaga. O lenei u'amea u'amea nickel e mafai ona fa'aaogaina i le tulaga e pei o le ueloina aua e tete'e i le fa'avaeina o carbide tuaoi o saito i totonu o le sone e a'afia i le vevela.

    O lenei u'amea nickel e maua ai le tete'e lelei i le hydrochloric acid i fa'atonuga uma ma le vevela. E le gata i lea, o Hastelloy B2 e sili ona tete'e atu i pitting, fa'alavelave fa'a'a'a'a ta'e ma le naifi-laina ma osofa'iga sone vevela. Alloy B e maua ai le tetee i le sulfuric acid mama ma le tele o mea e le faʻamaʻiina.

  • HASTELLOY B2 UNS N10665 W.NR.2.4617

    Hastelloy B2 o se vaifofo malosi faʻamalosia, nickel-molybdenum alloy, faʻatasi ai ma le tetee tele i le faʻaitiitia o siosiomaga e pei o le hydrogen chloride gas, ma sulfuric, acetic ma phosphoric acids. O le Molybdenum o le elemene faʻafefiloi muamua lea e maua ai le malosi o le pala i le faʻaitiitia o siosiomaga. O lenei u'amea u'amea nickel e mafai ona fa'aaogaina i le tulaga e pei o le ueloina aua e tete'e i le fa'avaeina o carbide tuaoi o saito i totonu o le sone e a'afia i le vevela.

    O lenei u'amea nickel e maua ai le tete'e lelei i le hydrochloric acid i fa'atonuga uma ma le vevela. E le gata i lea, o Hastelloy B2 e sili ona tete'e atu i pitting, fa'alavelave fa'a'a'a'a ta'e ma le naifi-laina ma osofa'iga sone vevela. Alloy B2 e maua ai le tetee i le sulfuric acid mama ma le tele o mea e le faʻamaʻiina.

  • Hastelloy

    Aluia maualuga le vevela Fa'aaega vaila'au Vasega CPS Mn Si Ni Cr Co Cu Fe N Mo Al WV Ti isi e le sili atu nai lo HastelloyB 0.05 0.04 0.03 1 1 fa'avae ≤1 ≤2.5 - 4~6 - 26~30 - - 0.2~0.4 - - Hastelloy -2 0.02 0.04 0.03 1 0.1 faavae ≤1 ≤1 - ≤2 - 26~30 - - - - HastelloyB-3 0.01 0.04 0.03 3 0.1 ≥65 1~3 ≥65 ~3 ≤ 2 ≤0.5 ≤ 3 ≤0.2 ≤0.2 - ...
  • Hastelloy C-276 FA'AMATALAGA FAAMATALAGA

    HASTELLOY C276, UNS N10276 o lo'o fa'apea o le u'amea nickel sili ona lelei e mafai ona maua. Alloy C-276 e sili atu le teteʻe atu i pitting, faʻamaʻi faʻamaʻi faʻamaʻi, aemaise lava mo le faʻaogaina i le maualuga o le vevela, mea faʻapitoa ma meaola faʻalaʻau faʻafefiloi ma mea leaga (e pei o le formic acid ma le acetic acid), ma le suasami faʻafefe siosiomaga.

  • Alloy 2205 Duplex Plate Stainless

    Sandmeyer Steel Company o loʻo i ai se suʻesuʻega tele o le 2205 duplex plate stainless steel i mafiafia mai le 3/16" (4.8mm) e oʻo i le 6" (152.4mm). O le malosi e maua ai e tusa ma le faaluaina o austenitic stainless steels, o lea e mafai ai e se tagata mamanu ona faʻasaoina le mamafa ma faʻatauvaʻa ai le uʻamea pe a faʻatusatusa i le 316L poʻo le 317L.