FA'AIGA 600 FA'AMATALAGA FA'AMATALAGA
Fa'atekinisi Bulletin
Fomu Oloa Avanoa: Paipa, paipa, i'a, fasi, ipu, pa lapotopoto, pa mafolafola, fa'amea fa'ameamea, hexagon, uaea ma vaega fa'asalalau.
NEL alloyEL fa'ameamea HX
INCONEL u'amea 22
Fa'ainumera Fa'ainumera % mo Inconel Alloy 600
UNS Tofiga | N06600 |
Inconel Alloy | 600 |
Nikeli (fa'aopoopo atu i le Cobalt) | 72 min. |
Chromium | 14.0 - 17.0 |
Uamea | 6.00 - 10.00 |
kaponi | 0.15 maualuga. |
Manganese | 1.0 maualuga. |
Sulfur | 0.015 maualuga. |
Silicon | 0.50 maualuga. |
Kopa | 0.50 maualuga. |
Fa'aaliga: E mafai ona fa'amaoti mai nei u'amea i fatuga fa'asaoi luga o se fa'atonuga fa'apitoa.
INCONEL alloy 600 ua fa'aigoaina e
UNS N06600
Werkstoff Numera 2.4816.
Ua fa'amaonia le u'amea i lalo o le Boiler and Pressure Vessel Code a le American Society of Mechanical Engineers. Ua fa'amaonia i lalo o le Vaega I (Power Boilers), Vaega III (Vaau Faaniukilia), ma le Vaega VIII (Va'a Fa'amalosi). O fa'amamafa fa'ataga fa'ataga o lo'o maua i le Vaega II, Vaega D. Vaega I o lo'o fa'asoaina e le Code Case 1827.
O'oto'o, Pa, Uaea ma Fa'atauga
ASTM B 166/ASME SB 166, ASTM B 564/ASME SB 564, ASME Code Cases 1827 ma N-253, SAE/AMS 5665 ma 5687, BS 3075NA14 ma 3076NA14, 17752, DIN 1775 ma le 3076 , ma 9725, MIL-DTL-23229, QQ-W-390.
Papatusi, Pepa ma Fa'ailoga
ASTM B 168/ASME SB 168, ASTM B 906/ASME SB 906, ASME Code Cases 1827 ma N-253, SAE/AMS 5540, BS 3072NA14 ma 3073NA14, DIN 17750, ISO 6208, DIN 17750, ISO 6208, ISO 6208
Paipa ma Pipa
ASTM B 167/ASME SB 167, ASTM B 163/ASME SB 163, ASTM B516/ASME SB 516, ASTM B 517/ASME SB 517, ASTM B 751/ASME SB 751, ASTM B 775/ASME SB9 /ASME SB 829, ASME.
Mataupu Code1827, N-20, N-253, ma le N-576, SAE/AMS 5580, DIN 17751, ISO 6207, MIL-DTL-23227.
Isi- ASTM B 366/ASME SB 366, DIN 17742, ISO 4955A, AFNOR NC15Fe